The mechanical properties are tested in the longitudinal direction.
1) If ReH is not applicable then Rp0.2 is used.
2) A80 value applies for thicknesses < 3.00 mm.
3) A5 value applies for thicknesses ≥ 3.00 mm.
4) For both longitudinal and transverse direction.
1) Impact testing according to EN ISO 148-1 is performed on thicknesses ≥ 6mm. The specified minimum value corresponds to a full-size specimen.
1) If the material is to be hot-dip galvanized according to category A or category B in EN 10149-2 this must be specified at the time of order.Other galvanizing classes with higher Si-content are available after agreement.
2) Sum of Nb, V and Ti = max 0.22%.
The steel is grain refined.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.
Show specs in:
You can improve the performance and reduce the weight of your equipment by upgrading from Strenx® 600MC to Strenx® 700MC. A 17% higher yield strength means a higher load-bearing capacity. Get in touch with our steel specialists at SSAB Tech Support or SSAB Knowledge Service Center for an update on upgrading.