Car seat frames and tracks made lighter, stronger, more durable

Car seat frames and tracks are taking advantage of higher strength steels to reduce weight and wall thicknesses while increasing strength and durability.

Backrest side members can be made thinner and lighter when formed from Docol® 1000DP.

Backrest side members can be made thinner and lighter when formed from Docol® 1000DP.

Thinnest possible solution for car seat backrest side member

Going from 800 dual phase steel to Docol® 1000DP meant this car seat OEM could reduce the backrest side member to just 0.8 mm thickness, reducing weight and materials.

Car seat tracks in Docol® CR1000DP provide increased static performance and brinelling resistance.

Car seat tracks in Docol® CR1000DP provide increased static performance and brinelling resistance.

Car seat tracks are 25% lighter, with improved brinelling resistance

Upgrading from HR 500 LA steel to Docol® CR1000DP in 1.6 mm thickness meant this Tier 1 car seat supplier could reduce the weight of its seat tracks by 25%. Plus, the new UHSS steel improves both the static performance and the brinelling resistance, increasing the car seat tracks’ durability.

Rear seat frame made with Docol® 1000DP tubes deliver 40% lighter performance.

Rear seat frame made with Docol® 1000DP tubes deliver 40% lighter performance.

40% weight savings with gigapascal seat frame tubes

For the frame of this rear car seat, switching from HC420LA steel to Docol® 1000 dual phase steel enabled a reduction in tube wall thickness, from 2 mm to 1.2 mm, reducing the weight from 3 kg to 1.8 kg – making it 40% lighter.

Docol® 800DP tube and Docol® Roll 1000 for the rear tube and side member frame, respectively.

 Docol® 800DP tube and Docol® Roll 1000 for the rear tube and side member frame, respectively.

Lightweight steels for car seat rear tube and cushion side members

This new design for a car seat bottom frame leveraged the light weight of both Docol® 800DP tube for the rear member and Docol® Roll 1000 for the cushion side member frame. Starting a new design with Docol® AHSS or UHSS steels is a strong way to position your car seat frames ahead of the competition.

This car seat track replaced the more expensive re-rolled steel with Docol® 800LA in 1.64 mm and 1.90 mm thicknesses.

This car seat track replaced the more expensive re-rolled steel with Docol® 800LA in 1.64 mm and 1.90 mm thicknesses.

Car seat tracks save costs by replacing re-rolled steel

The manufacturer of car seat tracks replaced costly re-rolled steel with Docol® 800LA in 1.64 mm and 1.90 mm thicknesses. Docol® advanced high strength steels have the potential to reduce costs throughout your car seat frame and track construction.

Docol® HR 355HE to 550HE grades help semi-fine blanking operations achieve intricate shapes that are virtually free of micro-cracks.

Docol® HR 355HE to 550HE grades help semi-fine blanking operations achieve intricate shapes that are virtually free of micro-cracks.

Solving edge cracking during the forming of mechanisms for car seat recliners

The semi-fine blanking operations used to form conventional hot-rolled steels into gears and other car seat recliner mechanisms are known to cause edge cracking, leading to higher scrap rates. SSAB developed High Edge (HE) Ductility grades to virtually eliminate these micro-cracks.

Car seat frame steel grade suggestions

Headrest tube: Tubes, Docol CR 600-800 DP

Upper cross member: Docol CR 800-1000 DP

Lower cross member: Docol CR 1000 DP

Rear tube: Tubes, Docol CR 600-800 DP

Seat pan: Docol CR 340-420 LA, Docol FORM 04 (CR4)

Seat track: Docol CR 800-1000 DP, Docol CR 800-1000 CP, Docol CR 800 LA

Cushion side member: Docol CR 800-1000 DP, Docol CR 800-1000 CP

Recliner: Docol HR 700 LA, Docol HR 800-1000 CP

Backrest side member: Docol CR 800-1000 DP, Docol CR 800-1000 CP

car seat structure

Get AHSS/UHSS samples – fast

In just one to two weeks, you can get trial samples of most of our commercially available AHSS/UHSS steel grades – plus some of our newest, not-yet-released steels.

Other automotive applications

Our steel grades serve specific design purposes and are chosen by designers for a wide range of automotive applications.

Related content

SSAB plans to accelerate its fossil-free steel conversion by 15 years

As evidenced by the dispatches that follow, the race for climate-neutral vehicles is shifting into high gear. SSAB’s Board has taken a policy decision to fundamentally transform Nordic strip production and accelerate the company’s green transition. The decision was taken against the background of strongly growing demand for fossil-free steel.

Read more

Complex phase (CP) steels for the highest hole expansion ratios

Complex phase steels have the highest — up to 75% — hole expansion ratios available from advanced high strength steels. Their high HER values provide excellent cold-forming properties for punched and stretched edges/flanges, as well as deep-drawn shapes. CP steels’ superior yield strengths are used for high crash-energy absorption, while their elevated UTS levels enable thinner walls for significant automobile weight reductions.

Read more
Copyright 2026