Extra-high-hardness armor with very good resistance against penetration.

Armox® 600T is used as an add-on protection plate or where weight is critical. Armox® 600T is available in thicknesses between 4 and 20 mm with a guaranteed hardness range of 570‑640 HBW.

Benefits of Armox® 600T include:

 

  • Market-leading steel protection
  • Superior workshop properties
  • Optimized solutions
  • Perfect hardness/toughness balance, for combined penetration and blast protection
  • Expertise in ballistic protection from SSAB

 

Armox® 600T is not intended for further heat treatment.

 

Mechanical Properties

Thickness
(mmin)
Thickness
(mmin)
4.0 - 20.00.157 - 0.787
Hardness
(HBW)
570 - 640

Mechanical Testing

Brinell hardness test according to EN ISO 6506-1 on each heat treatment individual.

Charpy impact test according to EN ISO 148 on each heat and thickness from 6 mm.

 

Ultrasonic testing

According to EN 10160 Class E3S3.

 

Impact Properties

Thickness
(mmin)
Thickness
(mmin)
4.0 - 20.00.157 - 0.787
Min impact energy for transversal testing,
Charpy V 10x10 mm test specimen 1)
12 J / -40 °C8 ft-lbs / -40 °F

1) Average of three tests. Transverse to rolling direction. Single value min. 70% of specified average. For plate thicknesses under 12 mm sub-size Charpy-V specimen are used. The specified minimum value is then propotional to the specimen cross-section.

 

 

Chemical Composition (ladle analysis)

C *)
(max %)
C *)
(max %)
0.47
Si *)
(max %)
0.70
Mn*)
(max %)
1.00
P
(max %)
0.010
S
(max %)
0.003
Cr*)
(max %)
1.5
Ni*)
(max %)
3.0
Mo*)
(max %)
0.70
B*)
(max %)
0.005

Tolerances

More details are given in SSAB brochure Armox® Guarantees or on www.ssab.com.

Thickness

Tolerances according to Armox® Thickness Guarantees.

Armox® Guarantees meet the requirements of EN 10029 Class C, but offers narrower tolerances.

Length and Width

Tolerances conform to EN 10029 or to SSAB´s standard after agreement.

Dimensional tolerances for plate with mill edge according to special agreement. 

Shape

Tolerances according to EN 10029.

Flatness

Tolerances according to Armox® flatness guarantees, which are more restrictive than EN 10029 Class N (steel type L).

Surface Properties

According to EN 10163-2 Class B, Subclass 3.

Delivery Conditions

The delivery condition is QT (Quenched and Tempered).

 

Delivery requirements can be found in SSAB’s brochure Armox® Guarantees or www.ssab.com.