    General Product Description

    GreenCoat Hiarc color coated steel is available in regular and matt finishes as well as with a shine effect. It is available in a wide range of colors inspired by Nordic nature.

    GreenCoat Hiarc offers the highest level of durability for faҫades and cassettes where demands are high. However, it can also be used in roofing applications.

    The regular and matt finish as well as the metallic colors have a long production experience resulting in good color and gloss consistency. The shine effect finish has a special appearance through a multilayer coating providing glittery, but colored appearance and excellent properties.

    GreenCoat Hiarc color coated steel possesses excellent weather resistance properties (Ruv5), corrosion resistance and tolerates forming well. However, if extended corrosion properties are required, such as for buildings near a coastline, we offer GreenCoat Hiarc Max.

    Since GreenCoat Hiarc products offer a coating containing fluorine, the surface stays cleaner compared to other products. The coating is also easy to clean due to the hard surface. If needed, strippable protective films are available for this product.

    The reverse side of the sheet is painted with a two-layer grey backside coating.

    GreenCoat Hiarc complies with current REACH regulations and is fully chromate-free.

    SSAB’s color coated steels are all manufactured according to EN 10169.

    GreenCoat and Hiarc are trademarks of the SSAB group of companies.

    Technical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Technical Properties Matt Regular Shine effect
      Gloss 4 35 1) 35
      Minimum inner bending radius 1 x sheet thickness 1 x sheet thickness 1 x sheet thickness
      Scratch resistance 30 N 30 N 35 N
      UV radiation resistance RUV5 RUV5 RUV5
      Corrosion resistance 2) RC4 RC4 RC5
      Stain resistance Excellent Excellent Excellent
      Highest operating temperature 110 °C 110 °C 110 °C
      Fire classification, EN 13501-1 A1 s1 d0 A1 s1 d0 A1 s1 d0
      Coating thickness, nominal (primer + top coat) 27 µm 27 µm 3) 40 µm
      Coating structure Structured Smooth Smooth glittery
      Steel designation 4) S280GD, S320GD, DX51D S280GD, S320GD, DX51D S280GD, S320GD, DX51D
      Zinc coating 275 g/m2 275 g/m2 275 g/m2
      Min steel thickness 4) 0.50 mm 0.50 mm 0.50 mm
      Steel width 4) 1000 - 1420 mm 1000 - 1500 mm 1000 - 1420 mm
      Compare parameters

      Select one parameter to compare

      Comparison

        1) For some metallic colors the target gloss is different.

        2) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

        3) Specific colors have higher nominal film thickness value than listed in the table to reach the targeted color.

        4) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

        Colors

        Below are the colors currently available. Other colors can be agreed upon separately.

        Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

        For information on thermal properties (solar reflectance index SRI or thermal emittance TE) of available colors, please contact SSAB Tech Support.

        29 Available Colors
        Preview colors
        Close

        Colors

        GreenCoat Hiarc

        Frost White

        RR106 / SS0009

        Regular

        Nordic White

        RR1H3 / SS0020

        Regular

        Winter White

        RR20 / SS0005

        Regular, Shine effect

        Fog White

        RR143 / SS----

        Regular

        Cloud Grey

        RR2B1 / SS----

        Regular

        Pebble Grey

        RR21 / SS0011

        Regular

        Stone Grey

        RR22 / SS0554

        Regular

        Rock Grey

        RR237 / SS0061

        Regular

        Anthracite Grey

        RR2H8 / SS0087

        Regular

        Mountain Grey

        RR23 / SS0036

        Regular, Matt

        Cliff Grey

        RR288 / SS0455

        Regular

        Slate Grey

        RR2H3 / SS0534

        Regular

        Nordic Night Black

        RR33 / SS0015

        Regular, Matt

        Walnut Brown

        RR32 / SS0387

        Regular, Matt

        Hazelnut Brown

        RR8H2 / SS0426

        Regular

        Almond Brown

        RR30 / SS0187

        Regular

        Cottage Red

        RR29 / SS0758

        Regular

        Tile Red

        RR750 / SS0760

        Regular

        Harvest Yellow

        RR24 / SS0189

        Regular

        Silver Fir Green

        RR5J3 / SS0975

        Regular

        Pine Green

        RR11 / SS0830

        Regular

        Lake Blue

        RR35 / SS0558

        Regular

        Ocean Blue

        RR4F8 / SS0510

        Regular

        River Blue

        RR34 / SS0557

        Regular

        Metallic Silver

        RR40 / SS0045

        Regular, Matt

        Metallic Dark Silver

        RR41 / SS0044

        Regular, Matt

        Metallic Titanium

        RR45 / SS----

        Regular, Matt

        Metallic Gold

        RR974 / SS0645

        Regular

        Metallic Copper

        RR979 / SS0778

        Regular

        Note for Metallic and all Matt colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size.

        Reverse Side Coating

        Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

        Hide/Show specific columns Edit
        Select columns to display
          Technical Properties
          Nominal Coating Thickness (primer + top coat) 12 µm
          Color Grey
          Corrosion Resistance Min CPI3
          Compare parameters

          Select one parameter to compare

          Comparison

            Technical Properties
            Nominal Coating Thickness (primer + top coat)
            12 µm
            Technical Properties
            Color
            Grey
            Technical Properties
            Corrosion Resistance
            Min CPI3

            For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production year is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

            Double Sided Products

            GreenCoat Hiarc, regular gloss is also available as a double sided product with non-metallic colors for reverse side. However, different sides of the sheet cannot be mixed due to the possibility of a visual difference. The reverse side may show wider variation in color and gloss.

            Protective Film

            Temporary protective films are available for protection during processing and installation. Protective films are applied on the top side of the Product. Films will be centered to the strip meaning that typically there are small unprotected areas in both edges of the strip. Unprotected area may be cut away if customer so wishes. Joined film strip ends are marked with red tape on the edge of the Product.

            Products with protective film should be stored in dry and warm conditions, since the adhesion between protective film and color coating decreases both in high and low temperatures. Humidity changes also the adhesion properties and in worst case leaves the adhesive part of the film on the Product surface.

            Adhesion of protective film increases over time, eventually making it difficult to remove the film from the Product’s surface. Due to that, protective film is recommended to be removed from the material as soon as possible, but no later than six months from the manufacturing of the Product or after one month from the end product installation depending on which comes first.

            Protective film decreases friction between coil windings, which creates a high risk of coil collapsing on thin gauge coils. Due to the risk of collapsing, SSAB does not recommend protective films for steel nominal thickness ≤ 0,60 mm. If protective film is essential, following precautions must be taken to minimize the risk of collapsing: Max coil weight < 5 tons and self-supporting coil protection shields must be used in the package.

            Typical protective film thickness is around 45µm, max working temperature +80°C and max and min stripping temperatures +40°C & -10°C.

            Protective film has a good resistance to forming but is susceptible to cuts. When working with material with a protective film, clean tools that do not damage the film, and appropriate methods are to be used. Cutting fluids are not needed because the film protects the material surface and reduces friction. Cutting fluids may also have negative impact on the protective film and its adhesion.

            Films used with GreenCoat Hiarc and GreenCoat Hiarc Max metallic colors have arrows indicating the painting direction of the strip, which enhances the use of the material in the manufacturing of end products.

            Protective films can be recycled as plastics, combusted or disposed via the municipal waste management system depending on the local waste management guidelines and regulations.

            Contact Information