1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.
2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.
3) FAX fulfills the requirements of EN 10346 DX51D, PLX fulfills the requirements of EN 10346 DX54D.
Below are the colors currently available. Other colors can be agreed upon separately.
Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.
Colors
GreenCoat RWS Pro
Nordic White
RR1H3 / SS0020
Regular
Winter White
RR20 / SS0005
Regular
Snow White
RR19 / SS0001
Regular
Pebble Grey
RR21 / SS0011
Regular
Stone Grey
RR22 / SS0554
Regular
Anthracite Grey
RR2H8 / SS0087
Regular
Mountain Grey
RR23 / SS0036
Regular
Ridge Grey
RR2F7 / SS0035
Regular
Nordic Night Black
RR33 / SS0015
Regular
Walnut Brown
RR32 / SS0387
Regular
Chestnut Brown
RR887 / SS0435
Regular
Acorn Brown
RR827 / SS0434
Regular
Cocoa Brown
RR8G2 / SS6056
Regular
Cottage Red
RR29 / SS0758
Regular
Brick Red
RR7F2 / SS0742
Regular
Pine Green
RR11 / SS0830
Regular
Metallic Silver
RR40 / SS0045
Regular
Metallic Dark Silver
RR41 / SS0044
Regular
The product especially in metallic colors may have slight tonal difference between batches and especially if the time of production differs significantly.
Same coating is applied on both sides of the sheet. Customers can specify the color separately for each side.
The technical properties apply for both sides. However, different sides of the sheet cannot be mixed due to the possibility of a visual difference. The reverse side may show wider variation in color and gloss.
Reverse side stamping is not applicable for double sided products.