Side-impact car door beams are a key component to “survival space” in automobiles during a crash. Leveraging higher strength steels for side-impact beams offers car OEMs a cost-efficient way to achieve 5-star crash safety performance.
Side-impact automobile collisions, in general, result in more severe injuries than other types of collisions. Severe injuries to both upper and lower body can occur if the survival space is inadequate. Using optimized designs and advanced high strength steel grades for side-impact beams can significantly increase survival space in cars, helping to protect drivers and passengers during side impact crashes.
For a new design for side-impact car door beams, a Tier 1 supplier needed to improve crash test performance, corrosion resistance, and cost efficiency – while lowering weight. Aluminum proved to be too costly, while press hardening steel would require investments in hot-forming presses, as well as slower production times.
Instead, the Tier 1 chose Docol® CR1500M-EG in 1.0 mm thickness. The martensitic 1500 MPa side-impact beams helped the car achieve a 5-star crash safety rating for side impacts while their 1.0 mm thickness kept the car door light in weight. Plus, the electrogalvanized metal coating provides the required level of corrosion resistance at a cost-efficient price point.
This new design for waistline car door side reinforcement features a roll-formed, laser-welded, closed profile beam in hot-dip galvanized Docol® HR700LA-GI. The waistline beam is either 2.0 mm or 3.0 mm thick, depending on the car model. With the high-strength, low-alloy (HSLA) 700 MPa steel, the waistline reinforcement beam achieves 5-star crash test performance and fulfills all current global automotive safety requirements.
The existing design for this side-impact car door beam used CR1200M-EG. To further improve its crash performance and to reduce weight, the OEM is doing trial stamping of Docol® CR1400M-EG in 1.3 mm thickness. In addition to achieving 5-star crash test performance, the beam can be stamped using conventional cold stamping processes, achieving better cost and energy efficiencies compared to hot-stamping or using aluminum.
Waistline reinforcement beam: HR 700LA – CR1700M
Side impact beam: CR1180DP – CR1700M – CR2000PHS


In just one to two weeks, you can get trial samples of most of our commercially available AHSS/UHSS steel grades – plus some of our newest, not-yet-released steels.