ASTM A514
Commercial steel

ASTM A514

The ASTM A514 specification is the Standard Specification for High-Yield-Strength, Quenched and Tempered Alloy Steel Plate, Suitable for Welding used in applications where Yield Strengths of ≥ 100 ksi are required for plates up to 2-1/2" thick, inclusive.  Plates > 2-1/2"  and ≤ 6" in thickness have a minimum Yield Strength requirement of 90 ksi.    Each grade has different chemistry requirements.  Typical applications include transport trailers, construction equipment, crane booms, mobile man-lifts, agricultural equipment, heavy vehicle frames and chassis, and welded bridge structural members.

PRODUCT NAME
USED FOR
DIMENSIONS
DATA SHEET
PRODUCT NAME
ASTM A514 Grade B
USED FOR

Structural

DIMENSIONS

T: 0.188 - 1.25 Inches

W: Up to 120 Inches

L: Up to 600 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A514 Grade E
USED FOR

Structural

DIMENSIONS

T: 0.185 - 6 Inches

W: Up to 132 Inches

L: Up to 590 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A514 Grade F
USED FOR

Structural

DIMENSIONS

T: 0.185 - 2.5 Inches

W: Up to 132 Inches

L: Up to 590 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A514 Grade H
USED FOR

Structural

DIMENSIONS

T: 1.251 - 2 Inches

W: Up to 120 Inches

L: Up to 600 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A514 Grade Q
USED FOR

Structural

DIMENSIONS

T: 0.185 - 6 Inches

W: Up to 590 Inches

L: Up to 590 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A514 Grade S
USED FOR

Structural

DIMENSIONS

T: 0.188 - 2 Inches

W: Up to 120 Inches

L: Up to 600 Inches

DATA SHEET

English