Patterned steel enhances grip, durability, and safety on walking surfaces, making it ideal for outdoor environments prone to freezing. Patterned steel is widely used in both dry industrial settings and challenging outdoor conditions.
The general name “Patterned steel” is used to mean all the patterns and both patterned coils and patterned cut length sheets. In everyday language patterned steel is often named in accordance with its most general use i.e. floor plate.
Patterned steels are used for enhancing the grip, durability and safety of walking surfaces. The properties of Tear Pattern T (European Tear) and Tear Pattern A (American Tear) are best suited for outdoor applications where the surface may be susceptible to freezing. Patterned steel can be supplied as cut length sheets or coils, either with mill edges or with sheared edges.

The Chequer Pattern R, which has excellent wear resistance properties, is recommended for dry environments. The properties of Tear Pattern T (European Tear) and Tear Pattern A (American Tear) are best suited for outdoor applications where the surface may be susceptible to freezing. Tear Pattern A (American Tear) is the best choice, however, for applications in which formability is required as the flangeability of this pattern is equally good in all sheet directions. The reference standards for patterned steels are DIN 59220/00, SEL014E-79, SFS-EN10363:2016 and ASTM A 786-15 (2021).








The dimensions of the patterns are:
Weight of patterned steels:
The smallest order is one patterned coil or the equivalent of one coil in the same width of cut lengths. Larger orders must be multiples of this minimum amount. Cut lengths of patterned sheet are supplied in bundles. Bundles always contain cut lengths of the same thickness, width and length. The tolerance on delivery weight of patterned coils and cut lengths is ±10 %, with a minimum of -2 tonnes and maximum of +3 tonnes. The recommended weight / width ranges for patterned coils and cut lengths are 8–12 kg/mm of width and 17–20 kg/mm of width. The weight/width range is calculated by dividing the weight of a ready-made coil in kilograms by its width in millimetres. The weight/width range of cut lengths is calculated from the original coil before it is cut to cut lengths.
Patterned steels are manufactured in three main strength categories of structural steel:
Patterned steels of other steel grades or other strength classes are manufactured when agreed upon separately.
The mechanical properties of patterned steel that are in compliance with standards ASTM A 786 and SFS-EN10363:2016 meet the requirements set for the steel grade in question. The elongation requirements for patterned steel in accordance with DIN 59220 must be checked, when necessary, from the supplier. The materials testing of patterned steel is carried out in accordance with the respective material and patterned steel standards
An inspection certificate EN 10204-3.1 is provided in accordance with the order requirements. Patterned steels are marked on order and drawing as shown in the following examples:
The values shown are for patterned coils and cut to length sheets with mill edges.
Strength class ReH = 235 MPa
| Thickness mm | Width mm |
|---|---|
| 3.00–3.49 | 1200–1535 |
| 3.50–3.99 | 1200–1660 |
| 4.00–4.74 | 1200–1710 |
| 4.75–10.00 | 1100–1860 |
| 10.01–13.00 | 1000–1585 |
Strength class ReH ≈ 275 MPa
| Thickness mm | Width mm |
|---|---|
| 3.00–3.49 | 1200–1360 |
| 3.50–3.99 | 1200–1485 |
| 4.00–4.74 | 1200–1530 |
| 4.75–5.99 | 1100–1710 |
| 6.00–10.00 | 1000–1710 |
| 10.01–13.00 | 1000–1535 |
Strength class ReH ≈ 355 MPa
| Thickness mm | Width mm |
|---|---|
| 3.50–3.99 | 1200–1335 |
| 4.00–4.74 | 1200–1430 |
| 4.75–4.99 | 1100–1530 |
| 5.00–5.99 | 1100–1660 |
| 6.00–10.00 | 1000–1660 |
| 10.01–13.00 | 1000–1410 |
For patterned steels with sheared edges the maximum width is reduced by 40 mm compared with the standard value of the corresponding thickness. Patterned cut length sheets may be supplied in the length range of 2,000–12,000 mm. The inside diameter of patterned coils is usually 760 mm, but coils with an inside diameter of 610 mm can be supplied on request.
Dimensions other than those shown in the tables can be supplied by special agreement.