Trailers and body builders

This new body design is made of Hardox® 450 and 500, increasing the dumper’s load capacity by about 11% compared to the original design. It is partly due to the redesign and upgrading of wear liners, saving approximately 80% of their weight.

SSAB EcoUpgraded

Together with our customers, SSAB continually upgrades steel and equipment designs. SSAB EcoUpgraded saves CO2 both in steel production and during the full lifetime of the machine.

From the CO2 payback time and onwards, every extra hour brings additional savings.

EcoUpgraded logo

Savings on CO₂

SSAB EcoUpgraded Dumper body
Calculation data
Fuel consumption, fully loaded40 litres/hour
Fuel consumption, without load20 litres/hour
Machine usage per year2 000 hours/year
Distance with maximum load60 %
Service lifetime10 years
Maximum payload (before upgrading)32 380 kg
Gross weight (fully loaded)63 440 kg
Weight of original parts7 200 kg
Weight of upgraded parts3 500 kg
Wear resistance steel saved during lifetime5 000 kg