ASTM A588 Grade B

Download data sheet

General Product Description

The ASTM A588 specification is the Standard Specification for High-Strength Low-Alloy Structural Steel , up to 50 ksi Minimum Yield Point, with Atmospheric Corrosion Resistance for applications where strength and durability are needed. The required ASTM G101 Corrosion Resistance Index must be ≥ 6.0. In addition to the typical application in welded bridges and buildings, the specification is also commonly used in passenger rail cars.

Available Dimensions

Grade
Grade
Grade B
Product type
Plate
Thickness
(inmm)
0.188 - 0.5004.78 - 12.7
Width
(inmm)
72 - 961800 - 2400
Length
(inmm)
240 - 7206100 - 18300
Grade
Grade
Grade B
Product type
Plate
Thickness
(inmm)
0.250 - 2.0006.35 - 50.80
Width
(inmm)
72 - 1201800 - 3050
Length
(inmm)
240 - 10206100 - 25910
Grade
Grade
Grade B
Product type
Plate
Thickness
(inmm)
2.01 - 4.9051.1 - 124
Width
(inmm)
72 - 131.91800 - 3350
Length
(inmm)
240 - 10206100 - 25910

Thickness: Please inquire plate thicknesses greater than the listed maxima.  

Width: Please inquire for plate widths less than 72 in. and plate widths greater than 120 in.

Length: Please inquire for plate lengths less than 240 in. and for lengths greater than the listed maxima.

 

Mechanical Properties

Tensile testing is performed in the transverse direction according to ASTM A6 requirements. The tensile property requirements are tablulated below:

Product type
Product type
Plate
Grade
Grade B
Thickness
(inmm)
0.188 - 4.004.78 - 102
Yield strength
(min ksi)
50
Tensile strength
(ksi)
70
Elongation in 2" 1)
(min %)
21
Elongation in 8" 1)
(min %)
18
Product type
Product type
Plate
Grade
Grade B
Thickness
(inmm)
4.01 - 4.90102 - 124
Yield strength
(min ksi)
46
Tensile strength
(ksi)
67
Elongation in 2" 1)
(min %)
21
Elongation in 8" 1)
(min %)
—

1) For plates wider than 24 in, the elongation requirement is reduced by two percentage points. See elongation requirement adjustments in the Tension Test section of Specification ASTM A6.