    ASTM A131 Grades AH36, DH36, and EH36 are higher-strength structural steels with a minimum specified yield strength of 51 ksi and specified minimum Charpy V-notch impact toughness properties.

    Applications

    Typical applications include shipbuilding and mobile offshore drilling units and structures

    Available Dimensions

    Hide/Show specific columns Edit
    Select columns to display
      Grade Product type Thickness
      (inmm)
      Width
      (inmm)
      Length
      (inmm)
      Grade AH36 Plate 0.251 - 2.006.38 - 50.8 72 - 129.91800 - 3299 240 - 10206100 - 25910
      Grade DH36 Plate 0.251 - 2.006.38 - 50.8 72 - 129.91800 - 3299 240 - 10206100 - 25910
      Grade EH36 Plate 0.251 - 3.946.38 - 100 72 - 129.91800 - 3299 240 - 5906100 - 15000
      Compare parameters

      Select one parameter to compare

      Comparison

        Thickness: Please inquire for AH36 and DH36 greater than 2.00 in. thick.

        Width: Please inquire for available plate widths for thicknesses less than 0.250 in. For plate thicknesses of 0.250 in. or greater inquire for widths less than 72 in. or over 120 in.

        Length: Please inquire for plate lengths <240 in.and greater than the listed maximum.

        Mechanical Properties

        Tensile testing is performed in the transverse direction.

        Hide/Show specific columns Edit
        Select columns to display
          Grade Thickness
          (inmm)
          Yield strength
          (min ksi)
          Tensile strength
          (ksi)
          Elongation in 2" 1)
          (min %)
          Elongation in 8" 2)
          (min %)
          Grade AH36 0.251 - 2.006.38 - 50.8 51 71 - 90 22 19
          Grade DH36 0.251 - 2.006.38 - 50.8 51 71 - 90 22 19
          Grade EH36 0.251 - 3.946.38 - 100 51 71 - 90 22 19
          Compare parameters

          Select one parameter to compare

          Comparison

            1) For plates over 3.5 in. in thickness, a deduction from the specified percentage elongation in 2 in. shall be made in accordance with ASTM A6 Elongation Requirement Adjustments.

            2) For plates less than 5/16 in. in thickness , a deduction from the specified 8” elongation percentage shall be made in accordance with ASTM A6 Elongation Requirement Adjustments.

            Impact Properties

            Hide/Show specific columns Edit
            Select columns to display
              Grade Thickness
              (inmm)
              Test temperature
              (°F)
              Min Longitudinal Average Energy 1)
              (ft-lbs)
              Min transverse average energy 1)
              (ft-lbs)
              AH36 0.251 - 2.006.38 - 50.8 32 25 17
              DH36 0.251 - 2.006.38 - 50.8 -4 25 17
              EH36 0.251 - 2.006.38 - 50.8 -40 25 17
              EH36 2.001 - 2.8050.83 - 71.1 -40 30 20
              EH36 2.801 - 3.9471.15 - 100 -40 37 25
              Compare parameters

              Select one parameter to compare

              Comparison

                1) Specimen orientation at the option of the manufacturer unless otherwise specified in the order.

                No more than one value below the specified minimum average energy, but no less than 70% of the specified minimum average energy value.

                Minimum average energy for full-size specimens. Refer to ASTM A131 for sub-size specimen energy requirements.

                Carbon Equivalent

                (wt %)
                Hide/Show specific columns Edit
                Select columns to display
                  Grade AH36 DH36 EH36 EH36
                  Thickness (inmm) 0.1875 - 2.004.762 - 50.8 0.1875 - 2.004.762 - 50.8 0.1875 - 2.004.762 - 50.8 2.001 - 3.9450.83 - 100
                  CEV (max %) 0.38 0.38 0.38 0.40