    ASTM A1018 is a standard specification for hot-rolled, heavy-thickness coils of carbon steel, commercial steel, drawing steel, structural steel, high-strength low-alloy steel and ultra-high strength steel. The specification covers steel coils in thicknesses of 0.230 in. to 1.000 in. A1018 Structural Steel (SS) Grade 36 has a specified minimum yield strength of 36 ksi.

    Available Dimensions

    Hide/Show specific columns Edit
    Select columns to display
      Grade Product type Thickness
      (inmm)
      Width
      (inmm)
      SS Grade 36 Type 2 Coils 0.230 - 0.6255.84 - 15.9 60 - 981500 - 2500
      Compare parameters

      Select one parameter to compare

      Comparison

        Width: Inquire for widths <60 in. down to 39.4 in.

        Mechanical Properties

        Tensile testing is performed in the longitudinal direction.

        Hide/Show specific columns Edit
        Select columns to display
          Grade Thickness
          (inmm)
          Yield strength
          (min ksi)
          Tensile strength
          (min ksi)
          Elongation in 2"
          (min %)
          Elongation in 8"
          (min %)
          SS Grade 36 Type 2 0.230 - 0.6255.84 - 15.9 36 58 21 18
          Compare parameters

          Select one parameter to compare

          Comparison

            Chemical Composition

            (Heat analysis, wt. %.)

            Hide/Show specific columns Edit
            Select columns to display
              Grade C
              (max %)
              Mn
              (max %)
              P
              (max %)
              S
              (max %)
              V
              (max %)
              Cb
              (max %)
              Ti
              (max %)
              N
              (max %)
              Cu 2)
              (max %)
              Ni 2)
              (max %)
              Cr 2)
              (max %)
              Mo 2)
              (max %)
              SS Grade 36 Type 2 0.25 1) 0.035 0.040 0.008 0.008 0.025 0.014 0.40 0.40 0.30 0.12
              Compare parameters

              Select one parameter to compare

              Comparison

                1) For product greater than 0.75 in. thick, the Mn is 0.80 to 1.20%. For each reduction of 0.01% below the specified carbon maximum, an increase of 0.06% Mn above the maximum is permitted to a maximum of 1.35%.

                2) Production only at “Limits B” for Cu, Ni, Cr, Mo.