    ASTM A1018 is a standard specification for hot-rolled, heavy-thickness coils of carbon steel, commercial steel, drawing steel, structural steel, high-strength low-alloy steel and ultra-high strength steel. The specification covers steel coils in thicknesses of 0.230 in. to 1.000 in. A1018 High-Strength Low-Alloy Steel (HSLAS) Grade 60 has a specified minimum yield strength of 60 ksi.

    Available Dimensions

    Hide/Show specific columns Edit
    Select columns to display
      Grade Product type Thickness
      (inmm)
      Width
      (inmm)
      HSLAS Grade 60 Class 1 Coils 0.230 - 0.6255.84 - 15.9 60 - 981500 - 2500
      Compare parameters

      Select one parameter to compare

      Comparison

        Width: Inquire for widths <60 in. down to 39.4 in.

        Mechanical Properties

        Tensile testing is performed in the transverse direction.

        Hide/Show specific columns Edit
        Select columns to display
          Grade Thickness
          (inmm)
          Yield strength
          (min ksi)
          Tensile strength
          (min ksi)
          Elongation in 2"
          (min %)
          Elongation in 8"
          (min %)
          HSLAS Grade 60 Class 1 0.230 - 0.6255.84 - 15.9 60 75 16 14
          Compare parameters

          Select one parameter to compare

          Comparison

            Chemical Composition

            (Heat analysis, wt. %.)

            Hide/Show specific columns Edit
            Select columns to display
              Grade C
              (max %)
              Mn
              (max %)
              P
              (max %)
              S
              (max %)
              Ti 1)
              (min %)
              V 1)
              (min %)
              Cb 1)
              (min %)
              Ni 2)
              (max %)
              Mo 2)
              (max %)
              Cu 2)
              (max %)
              Cr 2)
              (max %)
              HSLAS Grade 60 Class 1 0.26 1.50 0.04 0.04 0.005 0.005 0.005 0.40 0.12 0.40 0.30
              Compare parameters

              Select one parameter to compare

              Comparison

                1) One or more of Cb, V, and Ti may be added. When added the min for that element applies, if not added then there is no minimum requirement.

                2) Production only at “Limits B” for Cu, Ni, Cr, Mo.