ASTM A871
Commercial steel

ASTM A871

The ASTM A871 specification is the Standard Specification for High-Strength Low-Alloy Structural Steel Plates with Atmospheric Corrosion Resistance used in tubular structures and poles. Grades 60 and 65 are available in the as-rolled, normalized, or quenched and tempered delivery conditions as required to achieve the specified mechanical properties. The required ASTM G101 Corrosion Resistance Index must be ≥ 6.0.

PRODUCT NAME
USED FOR
DIMENSIONS
DATA SHEET
PRODUCT NAME
ASTM A871 Grade 60
USED FOR

Weathering Steel

DIMENSIONS

T: 0.138 - 2 Inches

W: Up to 120 Inches

L: Up to 1020 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A871 Grade 65
USED FOR

Weathering Steel

DIMENSIONS

T: 0.138 - 2 Inches

W: Up to 120 Inches

L: Up to 1020 Inches

DATA SHEET

English