ASTM A633
Commercial steel

ASTM A633

The ASTM A633 specification is the Standard Specification for Normalized High-Strength Low-Alloy Structural Steel Plates when superior notch toughness is needed at low temperatures. Grades C is available up to 4" in thickness and Grade E is available up to 6" in thickness. Typical applications are utility poles as plates, offshore platforms, construction equipment frames, electric shovel dipper handles and suspension components.

PRODUCT NAME
USED FOR
DIMENSIONS
DATA SHEET
PRODUCT NAME
ASTM A633 Grade C
USED FOR

Structural

DIMENSIONS

T: 0.375 - 3 Inches

W: Up to 123 Inches

L: Up to 600 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A633 Grade E
USED FOR

Structural

DIMENSIONS

T: 0.25 - 6 Inches

W: Up to 120 Inches

L: Up to 600 Inches

DATA SHEET

English