The ASTM A606 specification is the Standard Steel Specification for High-Strength, Low-Alloy, Hot Rolled and Cold Rolled Sheet and Strip Steel with Improved Atmospheric Corrosion Resistance for use in structural and other applications. A606 Type 4 steel has a minimum corrosion-resistance index of 6.0 based upon ASTM Guide G101.

ASTM A606 Type 4

ASTM A606 Type 4

USED FOR
DIMENSIONS
DATA SHEET
USED FOR

Weathering Steel

DIMENSIONS

T: 0.079 - 0.394 Inches

W: Up to 73 Inches