ASTM A573
Commercial steel

ASTM A573

ASTM A573 is a specification for structural quality carbon-manganese-silicon steel plates in three tensile strength ranges intended primarily for structural applications at atmospheric temperatures for which improved toughness is required. ASTM A573 Grade 70 has specified tensile strength range of 70-90 ksi.

A573 GR 70

A573 GR 70

USED FOR
DIMENSIONS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 0.1875 - 1.5 Inches

W: Up to 120 Inches

L: Up to 1020 Inches

DATA SHEET