ASTM A285
Commercial steel

ASTM A285

The ASTM A285 specification is the Standard Specification for Pressure Vessel Plates, Carbon Steel, Low- and Intermediate-Tensile Strength intended for fusion-welded pressure vessels.  Three grades having different strength levels are available in thicknesses up to 2", inclusively.

PRODUCT NAME
USED FOR
DIMENSIONS
DATA SHEET
PRODUCT NAME
A285 Grade A
USED FOR

Pressure Vessel

DIMENSIONS

T: 0.185 - 2 Inches

W: Up to 130 Inches

L: Up to 590 Inches

DATA SHEET

English

PRODUCT NAME
A285 Grade B
USED FOR

Pressure Vessel

DIMENSIONS

T: 0.1875 - 2 Inches

W: Up to 120 Inches

L: Up to 1020 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A285 Grade C
USED FOR

Pressure Vessel

DIMENSIONS

T: 0.1875 - 2 Inches

W: Up to 120 Inches

L: Up to 1020 Inches

DATA SHEET

English