SSAB Abrasion Resistant Commercial Steels are designed to maximize abrasion resistance while providing good formability and weldability. Each grade offers a minimum nominal hardness for use in moderate to heavy wear applications.
Show specs in:
Product Name | Dimensions | Datasheet |
|---|---|---|
| AR200 | T: 0.100 - 1.250 in L: 72 - 1020 in W: 48 - 103 inT: 2.54 - 31.75 mm L: 1800 - 25910 mm W: 1200 - 2620 mm | |
| AR235 | T: 0.188 - 0.750 in L: 72 - 1020 in W: 48 - 120 inT: 4.78 - 19.0 mm L: 1800 - 25910 mm W: 1200 - 3050 mm | |
| AR400F | T: 0.188 - 2.00 in L: 240 - 600 in W: 72 - 120 inT: 4.78 - 50.8 mm L: 6100 - 15200 mm W: 1800 - 3050 mm |
AR200
AR235
AR400F