Strenx 960 Plus

Strenx® 960 Plus

The high-strength structural steel at 960 MPa

Strenx® 960 Plus is a hot-rolled structural strip steel made for cold forming, with a minimum yield strength of 960 MPa.

Strenx® 960 Plus combines good weldability with good toughness and strength in the welds. These cut-to-length sheets feature excellent thickness accuracy in the strength level, providing an outstanding finish to the final products.

Typical applications include advanced lifting devices and lighter transport solutions and components.

Dimension Range

Strenx® 960 Plus is available as cut to length sheets in thicknesses of 2.0 - 8.0 mm. Strenx 960 Plus is available in widths up to 1600 mm and lengths up to 16000 mm depending on thickness. Please contact your sales representative for more information regarding dimensions.

 

Available Standards

EN 10025-6

EN 10051

EN 10163-2

Strenx® 960 Plus

Strenx® 960 Plus

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 0.08 - 0.31 Inches

W: Up to 62.99 Inches

L: Up to 629.92 Inches

STANDARDS

EN 10025-6

EN 10051

EN 10163-2

DATA SHEET