Strenx 1100 E/F

Strenx® 1100

The high-strength structural steel at 1100 MPa

Strenx® 1100 is a structural steel with a high yield strength at a minimum of 1100 MPa. Typical applications include demanding load-bearing structures.

Despite its strength, the material is surprisingly easy to weld and bend. Strenx® 1100 benefits include:

  • Good weldability with excellent HAZ strength and toughness
  • Exceptional consistency within a plate guaranteed by close tolerances
  • High impact toughness which provides for good resistance to fractures
  • Superior bendability and surface quality

Dimension Range

Strenx® 1100 E/F is available as plate in thicknesses of 4.0 – 40.0 mm. Strenx 1100 E/F is available in widths up to 3200 mm and lengths up to 14630 mm depending on thickness. More detailed information on dimensions is provided in the dimension program.

 

Available Standards

EN 10029

EN 10163-2

Strenx® 1100 E/F

Strenx® 1100 E/F

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

Low temperatures (down to -60°)

DIMENSIONS

T: 0.16 - 1.57 Inches

W: Up to 125.98 Inches

L: Up to 575.98 Inches

STANDARDS

EN 10029

EN 10163-2