Strenx 1100 CR

Strenx® 1100 CR

Cold-rolled structural steel at 1100 MPa

Strenx® 1100 CR is a cold-rolled structural steel with a minimum yield strength of 1100 MPa for stronger and lighter structures.

Typical applications include a wide range of components and parts in the lightest possible load-bearing structures, for example in the lifting sector.

Strenx® 1100 CR is available as cut-to-length sheets.

Dimension Range

Strenx® 1100 CR is available in thicknesses of 0.80 - 2.10 mm, widths up to 1500 mm and in lengths up to 8.5 meters, when delivered as cut-to-length sheets.

 

Available Standards

EN 10131

Strenx® 1100 CR

Strenx® 1100 CR

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 0.03 - 0.08 Inches

W: Up to 59.06 Inches

L: Up to 334.65 Inches

STANDARDS

EN 10131

DATA SHEET