Strenx 100 XF

Strenx® 100 XF

The cold-formable steel for light and heavy transportation components and solutions

Strenx® 100 XF is a thermomechanically rolled steel, made for cold forming, with a minimum yield strength of 100 ksi. It comes in coils, slit coils and cut-to-length sheets. Thickness measurements in inches can be found in the data sheet.

Strenx® 100 XF can be supplied in compliance with the requirements of ASTM A1011 or A1018 if agreed upon when you place your order.

Dimension Range

Strenx® 100 XF is available in thicknesses of 0.079 - 0.393 inches (2-10 mm), and in widths up to 63 inches (1600 mm) as coil, slit coil and as cut to length sheets in lengths up to 630 inches (16000 mm).
Strenx® 100 XF can be supplied according to ASTM A1011 or A1018 specifications if agreed up on at the time of order.

Available Standards

ASTM A1011

ASTM A1018

EN 10051

EN 10163-2 Class A, Subclass 3

Strenx 100 XF

Strenx 100 XF

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 0.08 - 0.39 Inches

W: Up to 62.99 Inches

L: Up to 629.92 Inches

STANDARDS

A1011

A1018

EN 10051

EN 10163-2 Class A, Subclass 3

DATA SHEET

English