Hardox HiTuf
Hardox HiTuf - Wear-resistant plate with extra-high toughness

Hardox® HiTuf

The extra-high tough steel for structural wear parts

Hardox® HiTuf is an abrasion-resistant plate with guaranteed impact toughness. With a nominal hardness of 350 HBW, it's a good choice for structural wear parts like thick cutting edges, demolition tools and rippers.

 

Order trial material Get free technical advice

Customer case-HiTuf a smashing success

Shredders made of HiTuf a smashing success

Customer case

Dimension Range

Hardox® HiTuf is available in thicknesses of  1.575 – 6.299". Hardox® HiTuf is available in widths up to 131.889" and lengths up to 575.984". For thicknesses over 4.921" preferred width is 64.960". More detailed information on dimensions is provided in the dimension program.

 

Available Standards

EN 10029

Hardox® HiTuf

Hardox® HiTuf

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Wear Resistant

DIMENSIONS

T: 1.575 - 6.299 Inches

W: Up to 131.89 Inches

L: Up to 575.98 Inches

STANDARDS

EN 10029

DATA SHEET