Hardox Extreme steel for extreme abrasion resistance

Hardox® Extreme

Hardox® Extreme steel for extreme abrasion resistance

Hardox® Extreme is the world's hardest wear plate with a nominal hardness of 60 HRC (Rockwell) and typical hardness of 650-700 HBW.

Hardox® Extreme is an abrasion resistant steel with a nominal hardness of 60 HRC, intended for applications with extreme high demands on abrasion resistance. Typical applications is liner plates, etc.

 

Order trial material Get free technical advice

Hardox wear steel for extreme abrasion resistance

Dimension Range

Hardox® Extreme is supplied in plate thickness of 0.314 - 0.748", up to 78.740" in width and up to 575.984" in length, preferred widths are 78.740 x 157.480", other width on request. More detailed information on dimensions is provided in the dimension program.

 

Available Standards

EN 10029

Hardox® Extreme

Hardox® Extreme

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Wear Resistant

DIMENSIONS

T: 0.315 - 0.748 Inches

W: Up to 78.74 Inches

L: Up to 575.98 Inches

STANDARDS

EN 10029

DATA SHEET