General Product Description

Duroxite® AP Wireis a gas shielded flux cored all positions hardfacing wire for components experiencing metal-to-metal wear, metal-to-earth wear, impact, and high abrasion applications. The deposit offers a good balance of impact and abrasion resistance. Deposits are forgeable, but can only be machined with special tools. The wire has been developed to operate in a smooth semi-spray transfer mode whilst welding in all positions. The deposited overlay is magnetic on carbon and low alloy steels but not on manganese steels.

Duroxite® AP Wire can be applied to carbon, low alloy, manganese, and other steel substrates.

Duroxite® AP Wire iis suitable for single and multiple-layer deposit up to three layers. Preheating, interpass temperature, and post-weld heat treatment are as needed according to base metal recommendations. If welding with downhill or uphill position, reduced wire feed speed and voltage are preferred to apply.

Key Benefits

  • Duroxite® AP Wire is a hardfacing wire for all positions welding.
  • The Duroxite® AP Wire deposited overlay consists of medium alloy martensite for good abrasion and impact resistance.

Typical Applications

Duroxite® AP Wire has many applications where moderate/high impact and high abrasion wear conditions prevail. Examples: Bucket teeth, tillage tools, bucket lips, bucket sides, cutting edges, sand dredge equipment, dragline buckets, conveyor chutes, grizzly bars, screw flights, metal shredders, sliding metal parts, tire shredder knives, extruder screws, tamper feet, churn drills, muller tires. Especially applicable for all-positional welding and re-instating of hardfacing sealing runs on clad wear plate fabrications.


Standard Dimensions

Hide/Show specific columns Edit
Select columns to display
    Standard diameter
    Imperial
    3/64" 1)
    1/16"
    Compare parameters

    Select one parameter to compare

    Comparison

      Standard diameter
      Imperial
      3/64" 1)
      Standard diameter
      Imperial
      1/16"

      1) 0.045"

      Mechanical Properties

      Hide/Show specific columns Edit
      Select columns to display
        Typical all-weld metal surface Hardness 1)
        Hardness: 2-layer deposit on mild steel Hardness: 3-layer deposit on mild steel
        55 - 59 HRC 56 - 60 HRC
        Compare parameters

        Select one parameter to compare

        Comparison

          Typical all-weld metal surface Hardness 1)

          Hardness: 2-layer deposit on mild steel
          55 - 59 HRC
          Typical all-weld metal surface Hardness 1)

          Hardness: 3-layer deposit on mild steel
          56 - 60 HRC
          1) Surface hardness is measured on machined flat surface just below overlay surface.

          Test results for mechanical properties

          Test results for mechanical properties, deposit overlay chemical composition and surface hardness were obtained from a weld produced and tested according to prescribed standards, and should not be assumed to be the expected results in a particular application or weldment. Actual results will vary depending on many factors, including, but not limited to, weld procedure, substrate chemistry and working temperature, weldment design and fabrication methods. Users are cautioned to confirm by qualification testing, or other appropriate means, the suitability of any welding consumable and procedure before use in the intended applications.

          Chemical Composition

          Hide/Show specific columns Edit
          Select columns to display
            Typical all-weld metal analysis (Weight %)
            C
            (%)
            Mn
            (%)
            Si
            (%)
            Cr
            (%)
            Mo
            (%)
            Fe
            0.4 1.0 0.5 5.5 0.5 Balance
            0.5 1.3 0.6 7.0 0.6 Balance
            Compare parameters

            Select one parameter to compare

            Comparison

              Welding recommendations

              Hide/Show specific columns Edit
              Select columns to display
                Welding conditions
                Current type Shielding gas Welding positions
                DCEP (Direct current electrode positive) 75% Ar + 25% CO2 gas mixtures All Positions including flat, horizontal, vertical, overhead
                Compare parameters

                Select one parameter to compare

                Comparison

                  Welding parameters recommendations

                  Hide/Show specific columns Edit
                  Select columns to display
                    Diameter
                    Amperage (A)
                    Voltage (V)
                    Stick-out
                    Imperial Range Optimum Range Optimum Range Optimum
                    3/64" 1) 170 - 275 220 24 - 30 28 1/2" - 1 3/16" 1"
                    1/16" 170 - 275 220 24 - 30 28 1/2" - 1 3/16" 3/4"
                    Compare parameters

                    Select one parameter to compare

                    Comparison

                      1) 0.045"

                      Recovery: 90%

                      Delivery Conditions

                      Hide/Show specific columns Edit
                      Select columns to display
                        Standard package
                        Diameter
                        Weight
                        Type Imperial Imperial
                        Spool 3/64" 1) 33 lbs
                        Spool 1/16" 33 lbs
                        Compare parameters

                        Select one parameter to compare

                        Comparison

                          1) 0.045"

                          Fabrication and Other Recommendations

                          The welded overlay components can be processed by welding, cutting, forming and machining. Specific recommendations can be found in the Duroxite® Product brochure or by consulting your local technical support representative.

                          Safety precautions

                          When welding or cutting Duroxite® products, gases and harmful fumes are produced that are chemically complex and difficult to classify. The major toxic component in the fumes is hexavalent chromium. The proper exhaust ventilation equipment and fume-extraction torches are recommended, as well as suitable protective clothing and respiratory protection for operators.