General Product Description

Duroxite® AP Electrode is a solid cored electrode designed for components experiencing metal-to-metal wear, metal-to-earth wear, impact and high abrasion applications. It has an extruded coating containing the alloy elements. The deposit offers a good balance of impact and abrasion resistance. Deposits are forgable, but can only be machined with special tools. Duroxite® AP Electrode has a good weldability and can be applied in all positions.

Duroxite® AP Electrode can be applied to carbon, low alloy, manganese steels and other steel substrates. Duroxite® AP Electrode is suitable for single and multiple-layer deposit up to three layers. Preheating, interpass temperature, and post-weld heat treatment are as needed according to base metal recommendations. If welding with downhill or uphill position, reduced wire feed speed and voltage are preferred to apply.

Key Benefits

  • Duroxite® AP Electrode is a hardfacing electrode for all positions welding.
  • The Duroxite® AP Electrode deposited overlay consists of medium alloy martensite for good abrasion and impact resistance.

Typical Applications

Duroxite® AP Electrode has many applications where moderate/high impact and high abrasion wear conditions prevail. Examples: Bucket teeth, tillage tools, bucket lips, bucket sides, cutting edges, sand dredge equipment, dragline buckets, conveyor chutes, grizzly bars, screw flights, metal shredders, sliding metal parts, tire shredder knives, extruder screws, tamper feet, churn drills, muller tires. Especially applicable for all-positional welding and re-instating of hardfacing sealing runs on clad wear plate fabrications.

Dimension Range

Hide/Show specific columns Edit
Select columns to display
    Standard diameter
    Imperial
    5/32"
    Compare parameters

    Select one parameter to compare

    Comparison

      Standard diameter
      Imperial
      5/32"

      Mechanical Properties

      Hide/Show specific columns Edit
      Select columns to display
        Typical all-weld metal surface Hardness 1)
        Hardness: 2-layer deposit on mild steel Hardness: 3-layer deposit on mild steel
        55 - 60 HRC 55 - 60 HRC
        Compare parameters

        Select one parameter to compare

        Comparison

          Typical all-weld metal surface Hardness 1)

          Hardness: 2-layer deposit on mild steel
          55 - 60 HRC
          Typical all-weld metal surface Hardness 1)

          Hardness: 3-layer deposit on mild steel
          55 - 60 HRC
          1) Surface hardness is measured on machined flat surface just below overlay surface.

          Test results for mechanical properties

          Test results for mechanical properties, deposit overlay chemical composition, surface hardness, and ASTM G65-A weight loss were obtained from a weld produced and tested according to prescribed standards, and should not be assumed to be the expected results in a particular application or weldment. Actual results will vary depending on many factors, including, but not limited to, weld procedure, substrate chemistry and working temperature, weldment design and fabrication methods. Users are cautioned to confirm by qualification testing, or other appropriate means, the suitability of any welding consumable and procedure before use in the intended applications.

          Chemical Composition

          Hide/Show specific columns Edit
          Select columns to display
            Typical all-weld metal analysis (Weight %)
            C
            (%)
            Mn
            (%)
            Si
            (%)
            Cr
            (%)
            Mo
            (%)
            Fe
            0.5 0.6 0.6 5.2 1.3 Balance
            Compare parameters

            Select one parameter to compare

            Comparison

              Welding recommendations

              Hide/Show specific columns Edit
              Select columns to display
                Welding conditions
                Current type Welding positions
                DCEP (Direct current electrode positive) All Positions including flat, horizontal, vertical, overhead
                Compare parameters

                Select one parameter to compare

                Comparison

                  Welding conditions

                  Current type
                  DCEP (Direct current electrode positive)
                  Welding conditions

                  Welding positions
                  All Positions including flat, horizontal, vertical, overhead

                  Welding parameters recommendations

                  Hide/Show specific columns Edit
                  Select columns to display
                    Diameter
                    Amperage (A)
                    Imperial Range Optimum
                    5/32" 140 - 220 170
                    Compare parameters

                    Select one parameter to compare

                    Comparison

                      Recovery: 90%

                      Delivery Conditions

                      Hide/Show specific columns Edit
                      Select columns to display
                        Standard package
                        Diameter
                        Weight
                        Type Imperial Imperial
                        Box 5/32" 44 lbs
                        Compare parameters

                        Select one parameter to compare

                        Comparison

                          Fabrication and Other Recommendations

                          The welded overlay components can be processed by welding, cutting, forming and machining. Specific recommendations can be found in the Duroxite® Product brochure or by consulting your local technical support representative.

                          Safety precautions

                          When welding or cutting Duroxite® products, gases and harmful fumes are produced that are chemically complex and difficult to classify. The major toxic component in the fumes is hexavalent chromium. The proper exhaust ventilation equipment and fume-extraction torches are recommended, as well as suitable protective clothing and respiratory protection for operators.