Docol® PHS 1500 press hardening

Download data sheet

General Product Description

Hardenable boron steel for the automotive industry. Available as both hot rolled and cold rolled. Docol PHS 1500 steels are specially developed for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as door impact beams, bumper systems and B- pillar reinforcements.

Dimension Range

Cold rolled / UC: thickness 0.70-3.00 mm, width up to 1500 mm.

Hot rolled / UC: thickness 2.00-12.00 mm, width up to 1600 mm.

Slit strip and cut to length sheets are available upon request.

Mechanical Properties

Docol PHS FH 1500

Standard
SSAB
Condition
Full Hard
Test direction
T
Typical elongation A80
(%)
4
Typical elongation A5
(%)
—

Docol PHS CR 1500 Annealed

Docol PHS HR 1500+A

Standard
SSAB
Condition
Annealed
Test direction
T
Typical elongation A80
(%)
25
Typical elongation A5
(%)
33

1) Properties depend on the process.

Chemical Composition (ladle analysis)

C
(%)
C
(%)
0.20 - 0.25
Si
(%)
0.15 - 0.35
Mn
(%)
1.00 - 1.35
P
(max %)
0.025
S
(max %)
0.005
Cr
(max %)
0.35
B
(%)
0.0020 - 0.0050

Tolerances

Cold rolled (UC): Tolerances in accordance to EN 10131.

Hot rolled (UC): Tolerances in accordance to EN 10051.

Customized dimensional and shape tolerances are available upon request.

Surface treatments

Uncoated (UC): available as oiled.

All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® PHS steel product offer

Docol® PHS 1500 press hardening

View product

Docol® PHS 1800 press hardening

View product

Docol® PHS 2000 press hardening

View product

Related content

AHSS trial material stock

Want to discover unique automotive applications for AHSS materials? Try new production methods? Or create lighter components that can improve fuel efficiency, crash-worthiness and sustainability?

Read more

Automotive steel applications

Docol® steel grades serve specific design purposes and are chosen by designers for a wide range of applications and used by OEMs and tier suppliers in millions of vehicles around the world.

Read more

Forming data for Docol® AHSS steels

Existing Docol® customers get 24/7 access to the forming data you need to help in your selection and simulation of automotive advanced high strength steels.

Read more
Copyright 2026