ASTM A1011 CS Type B

Download data sheet

General Product Description

ASTM A1011 is a standard specification for hot-rolled, steel sheet and strip and coils of carbon steel, structural steel, high-strength low-alloy steel, high-strength low-alloy steel with improved formability, and ultra-high strength steel. The specification covers steel sheet, strip, and coils in thicknesses less than 0.230 in. A1011 Commercial Steel Type B is produced to a specified chemical composition only.

Available Dimensions

Grade
Grade
CS Type B
Product type
Coils
Thickness
(inmm)
0.188 - 0.2294.78 - 5.82
Width
(inmm)
60 - 981500 - 2500

Chemical Composition

(Heat analysis, wt %.)

Grade
Grade
CS Type B
C
(max wt %)
0.15
Mn
(max wt %)
0.60
P
(max wt %)
0.03
S
(max wt %)
0.035
Ti 1)
(max wt %)
0.025
Cb
(max wt %)
0.008
Ni
(max wt %)
0.20
Mo
(max wt %)
0.06
Cu 2)
(min wt %)
0.20
Cr
(max wt %)
0.15
V
(max wt %)
0.008

1) For steels containing 0.02% carbon or more, Ti is permitted to the lesser of 3.4N + 1.5S or 0.025%.

2) Copper steel with 0.20% minimum Cu.

Show specs in: