Docol® Tube 980DP
Provides advanced high strength and energy absorption
Docol® Tube 980 is advanced high-strength precision tube. Available in circular, it comes with different coating and surface options including cold rolled, galvanized, galvannealed and galfan. Customized shapes and other tailoring options are available upon request. Typical uses include automotive safety parts, where lightness and energy absorption are important.
Docol® Tube 980DP is manufactured by cold forming and high-frequency welding from clean, high-quality SSAB steel by modern and efficient tube lines.