ASTM A572
Commercial steel

ASTM A572

The ASTM A572 specification is the Standard Specification for High-Strength Low-Alloy Columbium-Vanadium Structural Steel for plates, structural shapes, sheet pilings and bars. ASTM A572 includes five grades with specified minimum yield strengths of 42, 50, 55, 60, and 65 ksi, respectively.  For applications where notch toughness is important, consult SSAB for specific Charpy V-notch toughness requirements.  ASTM A572 grades are used in a wide variety of structural applications in many market segments.

PRODUCT NAME
USED FOR
DIMENSIONS
DATA SHEET
PRODUCT NAME
ASTM A572 Grade 42
USED FOR

Structural

DIMENSIONS

T: 0.1 - 6 Inches

W: Up to 132 Inches

L: Up to 1020 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A572 Grade 50
USED FOR

Structural

DIMENSIONS

T: 0.1 - 4 Inches

W: Up to 132 Inches

L: Up to 1020 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A572 Grade 55
USED FOR

Structural

DIMENSIONS

T: 0.1 - 2 Inches

W: Up to 120 Inches

L: Up to 1020 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A572 Grade 60
USED FOR

Structural

DIMENSIONS

T: 0.1 - 1.25 Inches

W: Up to 120 Inches

L: Up to 1020 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A572 Grade 65
USED FOR

Structural

DIMENSIONS

T: 0.1 - 1.25 Inches

W: Up to 120 Inches

L: Up to 1020 Inches

DATA SHEET

English