The ASTM A387 specification is the Standard Specification for Pressure Vessel Plates, Alloy Steel, Chromium-Molybdenum plates used in the application of welded boilers and pressure vessels subjected to elevated temperatures. The two grades SSAB produces are available as Class 1 and/or Class 2.
Product Name | Dimensions | Datasheet |
|---|---|---|
| ASTM A387 Grade 11 | T: 0.185 - 3.60 in L: 73 - 590 in W: 60 - 131.9 in | |
| ASTM A387 Grade 12 | T: 0.276 - 2.00 in L: 154 - 590 in W: 75 - 129.9 in | |
| ASTM A387 Grade 22 | T: 0.185 - 3.60 in L: 73 - 590 in W: 60 - 131.9 in |