ASTM A131
Commercial steel

ASTM A131

The ASTM A131 specification is the Standard Specification for Structural Steel plates primarily used in ship construction. Steel grades covered in this specification require CVN Impact testing and are classified by minimum Yield Strengths. Grades classified as Ordinary Strength have a minimum Yield Strength of 34 ksi and grades classified as Higher Strength have a minimum Yield Strength of 46 ksi. The Condition of Supply is determined by the ordered thickness and product type ( plate, shapes and bars).

PRODUCT NAME
USED FOR
DIMENSIONS
DATA SHEET
PRODUCT NAME
A131 GR A, B, D & E
USED FOR

Structural

DIMENSIONS

T: 0.1875 - 3.94 Inches

W: Up to 130 Inches

L: Up to 1020 Inches

DATA SHEET

English

PRODUCT NAME
A131 GR AH/DH 32
USED FOR

Structural

DIMENSIONS

T: 0.251 - 1.5 Inches

W: Up to 120 Inches

L: Up to 1020 Inches

DATA SHEET

English

PRODUCT NAME
A131 GR AH/DH/EH 36
USED FOR

Structural

DIMENSIONS

T: 0.251 - 3.94 Inches

W: Up to 1299 Inches

L: Up to 1020 Inches

DATA SHEET

English