Coils for Conversion
Commercial steel

As-rolled Coil Product for Conversion to Plate Grades

In addition to SSAB producing coils to the ASTM 1011 and ASTM 1018 specifications, SSAB also produces As-rolled coils that can be converted by a coil processor to the requirements of the ASTM structural and pressure vessel steels specifications, and SSAB's proprietary specifications.  Inquire for other specifications and grades not listed in the table below, for example, CSA or API grades.  SSAB will only certify the As-rolled coils to the chemistry requirements of the respective specification.

PRODUCT NAME
USED FOR
DIMENSIONS
DATA SHEET
PRODUCT NAME
ASTM A572 Grade 42
USED FOR

Structural

DIMENSIONS

T: 0.1 - 6 Inches

W: Up to 132 Inches

L: Up to 1020 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A572 Grade 50
USED FOR

Structural

DIMENSIONS

T: 0.1 - 4 Inches

W: Up to 132 Inches

L: Up to 1020 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A572 Grade 55
USED FOR

Structural

DIMENSIONS

T: 0.1 - 2 Inches

W: Up to 120 Inches

L: Up to 1020 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A572 Grade 60
USED FOR

Structural

DIMENSIONS

T: 0.1 - 1.25 Inches

W: Up to 120 Inches

L: Up to 1020 Inches

DATA SHEET

English

PRODUCT NAME
ASTM A572 Grade 65
USED FOR

Structural

DIMENSIONS

T: 0.1 - 1.25 Inches

W: Up to 120 Inches

L: Up to 1020 Inches

DATA SHEET

English