Strenx 960 E/F

Strenx™ 960

The high-strength structural steel at 960 MPa

Strenx™ 960 is a structural steel that guarantees a minimum yield strength of up to 960 MPa depending on thickness.

Strenx™ 960 meets the requirements of EN 10 025-6 for the S960 QL grade and thicknesses. Typical applications include demanding load-bearing structures. 

Strenx™ 960 benefits include:

  • Exceptional consistency within a plate guaranteed by close tolerances
  • High impact toughness which provides for good resistance to fractures
  • Superior bendability and surface quality
  • Weldability with excellent HAZ strength and toughness


Dimension Range

Strenx® 960 E is available in 4.0 - 120.0 mm thickness and 960 F in 4.0 - 100.0 mm. Both grades are available in widths up to 3350 mm and lengths up to 14630 mm depending on thickness. More detailed information on dimensions is provided in the dimension program.

Available Standards

EN 10025-6

EN 10029

EN 10163-2

Strenx® 960 E/F

Strenx® 960 E/F

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 0.16 - 4.72 Inches

W: Up to 131.89 Inches

L: Up to 575.98 Inches

STANDARDS

EN 10025-6

EN 10029

EN 10163-2

DATA SHEET