Strenx 960 CR

Strenx™ 960 CR

The high-strength structural steel at 960 MPa

Strenx™ 960 CR is a cold-rolled structural steel with a minimum yield strength of 960 MPa used to produce stronger and lighter structures.

Typical applications include a wide range of components and parts, for example load-bearing structures. Strenx™ 960 CR comes in cut-to-length sheets.

Dimension Range

Strenx® 960 CR is available in thicknesses of 0.80-2.10 mm, widths up to 1500 mm and in lengths up to 8.5 meters, when delivered as cut-to-length sheets.

 

Available Standards

EN 10131

Strenx® 960 CR

Strenx® 960 CR

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 0.03 - 0.08 Inches

W: Up to 59.06 Inches

L: Up to 334.65 Inches

STANDARDS

EN 10131