Strenx™ 900
The high-strength structural steel at 900 MPa
Strenx™ 900 is a structural steel that guarantees a minimum yield strength of up to 900 MPa depending on thickness.
Strenx™ 900 provides a unique combination of strength and toughness together with first-rate workshop properties. Typical applications include load-bearing structures, where low weight is needed.
Strenx™ 900 meets the requirements of EN 10 025-6 for the S890 grade and thicknesses. Strenx™ 900E (complies with S 890 QL) is available in plate thicknesses of 4–100 mm, while Strenx™ 900F (complies with S 890 QL1) is available in the thickness range up to 80 mm.
Benefits include:
- High impact toughness which provides for good resistance to fractures
- Superior bendability and surface quality
- Weldability with excellent HAZ strength and toughness
- Exceptional consistency within a plate guaranteed by close tolerances