Strenx 700 MC

The high-strength structural steel at 700 MPa

Strenx™ 700 MC is a hot-rolled structural steel made for cold forming, with a minimum yield strength of 700 MPa for stronger and lighter structures.

Strenx 700 MC meets or exceeds the requirements of S700MC in EN 10149-2. Typical applications include a wide range of components and parts in demanding load-bearing structures.

Strenx 700 MC comes in coils, slit coils or cut-to-length sheets.

Dimension Range

Strenx® 700MC D/E is available in thicknesses of 2.00-10.00 mm and widths up to 1600 mm as coils, slit coils or cut to length sheets in lengths up to 16 meters.

 

Available Standards

EN 10051

EN 10163-2

EN 10149-2

Strenx® 700MC D/E

Strenx® 700MC D/E

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 0.08 - 0.39 Inches

W: Up to 62.99 Inches

L: Up to 629.92 Inches

STANDARDS

EN 10051

EN 10163-2

EN 10149-2

DATA SHEET