Strenx™ 1300
The ultra-high-strength steel at 1300 MPa
Strenx™ 1300 is an ultra-high-strength structural steel with a minimum yield strength of 1300 MPa.
Typical applications include load-carrying structures that place very high demands on low weight. SSAB developed Strenx™ 1300 for building the lightest possible steel solutions or providing an alternative to other materials.
Strenx™ 1300 benefits include:
- Good weldability with excellent HAZ strength and toughness
- Exceptional consistency within a plate guaranteed by close tolerances
- High impact toughness which provides for good resistance to fractures
- Superior bendability and surface quality