Strenx 110 XF

Strenx™ 110 XF

The thermomechanically rolled steel for cold forming

Strenx™ 110 XF is a thermomechanically rolled steel at 110 ksi made for cold forming and used for light and heavy transportation components and solutions.  It comes in coils, slit coils and cut-to-length sheets.

Thickness measurements in inches can be found in the data sheet. 

Dimension Range

Strenx® 110 XF is available in thicknesses of 0.079 - 0.393 inches (2-10 mm), and in widths up to 63 inches (1600 mm) as coil, slit coil and cut to length sheets in lengths up to 630 inches (16000 mm).

Available Standards

EN 10051

EN 10163-2 Class A, Subclass 3

Strenx 110 XF

Strenx 110 XF

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 0.08 - 0.39 Inches

W: Up to 62.99 Inches

L: Up to 629.92 Inches

STANDARDS

EN 10051

EN 10163-2 Class A, Subclass 3

DATA SHEET

English