SSAB Domex 500ML

SSAB Domex® 500ML

A high-strength, thermomechanically rolled steel at 500 MPa

SSAB Domex® 500ML is a thermomechanically rolled steel with a minimum yield strength of 500 MPa.

SSAB Domex® 500ML structural steel is easy to weld, bend and process in workshops and on site. Its high strength and good flangeability allow steel structures to be made using thinner steel plates and reduce number of welded joints. Environmentally sound, durable and smart structures are guaranteed using this high-strength, thermomechanically rolled (M) and low temperature (L) tough structural steel grade.  SSAB Domex® 500ML has no equivalence in any structural standard.

Dimension Range

SSAB Domex 500ML is available in thicknesses of 8.00-60.00 and in widths up to 3300mm depending on the thickness. More detailed dimensions are provided in the dimension program.

Available Standards

EN 10029

SSAB Domex 500ML

SSAB Domex 500ML

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 0.31 - 2.36 Inches

W: Up to 129.92 Inches

L: Up to 590.55 Inches

STANDARDS

EN 10029