SSAB Domex 315MC

SSAB Domex® 315MC

The hot-rolled, cold-forming steel at 315 MPa

SSAB Domex® 315MC is a hot-rolled, high-strength low-alloy (HSLA) steel that features consistent quality and excellent engineering properties.

Part of the SSAB Domex® range of steels, the SSAB Domex® 315MC grade is produced under rigorous quality control. A well-balanced analysis with a fine grain structure produced through thermomechanical rolling creates a steel with first-class mechanical and cold-forming properties.

Together with the steel’s high purity, these properties make for outstanding repeatability, excellent bending and cutting characteristics and a steel that can be welded using all standard methods.

This makes SSAB Domex® 315MC the ideal choice when looking for high productivity and high-quality end products. Typical applications include a wide range of fabricated components and steel structures.

SSAB Domex® 315MC meets or exceeds the requirements of S315MC in EN 10149-2. Upon agreement, it can be delivered as double certified. This double certification will enable producers of steel structures, in accordance with EN 1090, to use SSAB Domex® 315MC in their CE-marked final component or structure.

Dimension Range

SSAB Domex 315MC is available in thicknesses of 1.80-18.00 mm and widths up to 1860 mm as coils, slit coils and as cut to length in lengths up to 16 meters.

Available Standards

EN 10051

EN 10149-2

SSAB Domex 315MC

SSAB Domex 315MC

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 0.07 - 0.71 Inches

W: Up to 73.23 Inches

L: Up to 629.92 Inches

STANDARDS

EN 10051

EN 10149-2

DATA SHEET