A steel for pressing, forming and bending

SSAB Domex® 260LA is a high-strength, low-alloy steel intended for general presswork, bending and forming. Typical applications include bent profiles.

SSAB Domex® 260LA offers consistent properties that assist modern, rapid production methods.

SSAB Domex 260LA is available in thicknesses of 0.50-3.00 mm and widths up to 1500 mm as coils, slit coils and as cut to length in lengths up to 8.5 meters.

Available Standards

EN 10131

EN 10268