SSAB Domex® 240YP

The hot-rolled structural steel for cold forming at 240 MPa

SSAB Domex® 240YP is a hot-rolled structural steel that features consistent quality and excellent engineering properties.

Part of the SSAB Domex® range of steels, the SSAB Domex® 240YP grade is produced under rigorous quality control. A well-balanced analysis with a fine grain structure produced through thermomechanical rolling creates a steel with first-class mechanical and cold-forming properties.

Together with the steel’s high purity, these properties make for outstanding repeatability, excellent bending and cutting characteristics and a steel that can be welded using all standard methods.

This makes SSAB Domex® 240YP the ideal choice when looking for high productivity and high-quality end products. Typical applications include a wide range of fabricated components and steel structures.

SSAB Domex® 240YP meets or exceeds the requirements of S235JRC, S235J0C or S235J2C in EN 10025-2, depending on agreed impact strength requirements at the time of order. Upon agreement, it can be delivered double certified and CE marked.

Dimension Range

SSAB Domex 240YP is available in thicknesses of 1.80-20.00 mm and widths up to 1860mm depending on thickness as coils, slit coils and as cut to length in lengths up to 16 meters.

Available Standards

EN 10051

SSAB Domex 240YP

SSAB Domex 240YP

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 0.07 - 0.79 Inches

W: Up to 73.23 Inches

L: Up to 629.92 Inches

STANDARDS

EN 10051