GreenCoat Mica BT
Proven durability that outlasts the harshest weather.
GreenCoat Mica BT color coated steel is available in an exclusive, glittery matt textured finish. It uses a patented bio-based coating having Swedish rapeseed oil instead of traditional fossil oil in the paint, which is unique on the market. SSAB holds a worldwide patent for this coating technology (Bio-based Technology, BT).
GreenCoat Mica BT color coated steel offers a high level of durability for profiled roof tiles and profiles with high aesthetic demands. GreenCoat Mica BT possesses good gloss retention and color fastness and provides good protection against corrosion (RC5 class).
The reverse side of the sheet is painted with a two-layer grey backside coating.
GreenCoat Mica BT complies with current REACH regulations and is fully chromate-free.
SSAB’s color coated steels are all manufactured according to EN 10169.