ASTM A871 Grade 60

Download data sheet

General Product Description

The ASTM A871 specification is the Standard Specification for High-strength Low-Alloy Structural Steel Plate with Atmospheric Corrosion Resistance for plates used in tubular structures and poles. Grade 60 may be provided in the as-rolled, normalized, or quenched and tempered delivery condition as required to achieve the specified mechanical properties. The required ASTM G101 Corrosion Resistance Index must be ≥ 6.0.

Dimension Range

Grade
Grade
60
Product type
Mill Plate
Thickness
(in)
0.500 - 2.00
Width
(in)
72 - 120
Length
(in)
120 - 1020
Grade
Grade
60
Product type
Temper Leveled Plate
Thickness
(in)
0.138 - 0.500
Width
(in)
48 - 96
Length
(in)
72 - 720
Grade
Grade
—
Product type
Coil for Conversion To
Thickness
(in)
0.188 - 0.500
Width
(in)
72 - 96
Length
(in)
—

Mill plate: Please inquire for plate thicknesses of 0.375 inches up to 0.499 inches and greater than 1.25 inches, for plate widths less than 72 inches and greater than 120 inches, and for plate lengths less than 120 inches and greater than 1020 inches.

Temper Leveled Plate: SSAB's Cut-To-Length facilities use the temper leveled coil (TLC) process to produce temper leveled plate products. For additional information concerning our temper leveling process, please refer to our SSAB Americas: North American Cut-to-Length Operations brochure located under the Downloads section of our Commercial Steels Overview page.

Temper Leveled Plate Thickness: Inquire for thicknesses greater than 0.500 inches and up to 0.625 inches.

Coil for Conversion To: Coils are excluded from qualification to this specification until they are processed into a finished plate product and all required processing, inspections, and testing are performed. Coils For Conversion To product will be certified to chemistry only. Coils will be subject to availability, so please inquire.

Coil for Conversion To: Please inquire for coil thicknesses greater than 0.500 inches and for coil widths less than 72 inches and greater than 96 inches. Slitting capabilities are determined by strength levels and thicknesses, so please inquire all slit coil opportunities.

Mechanical Properties

Tensile testing is performed in the tranverse direction. The required tensile properties are tabulated below:

Grade
Grade
60
Thickness
(in)
0.138 - 2.00
Yield strength
(min ksi)
60
Tensile strength
(min ksi)
75
Elongation in 2" 1)
(min %)
18
Elongation in 8" 1)
(min %)
16

1) For plates wider than 24 in., the elongation requirement is reduced two percentage points. Additional elongation requirement adjustments are allowed per the Tension Tests section of Specification ASTM A6.

Impact Properties

Grade
Grade
60
Thickness
(in)
0.138 - 2.000
Minimum Longitudinal Average Absorbed Energy 1)
(ft-lbs)
15
Test temperature
(°F)
-20

1) CVN impact testing in accordance with ASTM A673.
Please inquire for orders requiring CVN impact testing.

Tolerances

Tolerances for Mill Plate:

Thickness, width and length tolerances for A871, Grade 60 plates are in accordance with ASTM A6. ASTM A6 Standard Flatness tolerances are available for all plate thicknesses.

Tolerances for Temper Leveled Plate:

Thickness, width and length tolerances for A871 Grade 60 plates are in accordance with ASTM A6. ASTM A6 Half-Standard Flatness tolerances or better are available for temper leveled plates. Flatness capabilities are determined bythe processing line and the minimum yield strength of the material.

Tolerances for Coils for Conversion To:

For minimum gauge orders, thickness and width tolerances are in accordance with the respective ASTM specifications of A568 for thicknesses of less than 0.230 inches(exclusive), and A635 for thicknesses of 0.230 inches to 1.00 inch, inclusive. Thickness tolerances are in accordance with Table S1.1 found in each of the ASTM specifications of A635 and A568, respective of thickness. Width tolerances are in accordance with Table 6 of ASTM A568 and Table 3 of ASTM A635. Thickness tolerances for nominal gauge orders must be inquired.
All tolerances will be confirmed to the customer via SSAB's Order Acknowledgement document.