EN 10149-2
EN 10149-2 is the European Standard for hot-rolled flat products made of high yield strength thermo-mechanically rolled steels for cold forming.
EN 10149-2 is the European Standard for hot-rolled flat products made of high yield strength thermo-mechanically rolled steels for cold forming.
Steels encompassed by this specification have minimum yield strengths ranging from 315 MPa to 460 MPa for thicknesses ranging from 1.5 mm up to 20 mm. The specification also covers steel grades having minimum yield strengths of 500 to 700 MPa in thicknesses of 1.5 to 16 mm.
The Product Data Sheet is currently under development. Please contact your Regional Sales Manager or Inside Sales Representative for our capabilities.