ASTM A1011 SS Grade 36

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

    Show specs in Imperial Metric

    General Product Description

    ASTM A1011 is a standard specification for hot-rolled, steel sheet and strip and coils of carbon steel, structural steel, high-strength low-alloy steel, high-strength low-alloy steel with improved formability, and ultra-high strength steel. The specification covers steel sheet, strip, and coils in thicknesses less than 0.230 in. A1011 Structural Steel (SS) Grade 36 has a specified minimum yield strength of 36 ksi.

    Available Dimensions

    Hide/Show specific columns Edit
    Select columns to display
      Grade Product type Thickness
      (inchesmm)
      Width
      (inchesmm)
      SS Grade 36 Type 2 Coils 0.188 - 0.2294.78 - 5.82 60 - 981500 - 2500
      Compare parameters

      Select one parameter to compare

      Comparison

        Thickness: Inquire for thicknesses <0.188 in. down to 0.079 in.

        Width: Inquire for widths <60 in. down to 39.4 in.

        Mechanical Properties

        Tensile testing is performed in the longitudinal direction.

        Hide/Show specific columns Edit
        Select columns to display
          Grade Product type Thickness
          (inchesmm)
          Yield strength
          (min ksi)
          Tensile strength
          (ksi)
          Elongation in 2"
          (min %)
          Elongation in 8"
          (min %)
          SS Grade 36 Type 2 Coils 0.188 - 0.2294.78 - 5.82 36 58 - 80 21 16
          Compare parameters

          Select one parameter to compare

          Comparison

            Chemical Composition

            (Heat analysis, wt. %.)

            Hide/Show specific columns Edit
            Select columns to display
              Grade C
              (max %)
              Mn
              (max %)
              P
              (max %)
              S
              (max %)
              Ti
              (max %)
              Cb
              (max %)
              Ni
              (max %)
              Mo
              (max %)
              Cu 1)
              (min %)
              Cr
              (max %)
              V
              (max %)
              SS Grade 36 Type 2 0.25 1.35 0.035 0.04 0.025 0.008 0.20 0.06 0.20 0.15 0.008