ASTM A1011 CS Type B

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

    Show specs in Imperial Metric

    General Product Description

    ASTM A1011 is a standard specification for hot-rolled, steel sheet and strip and coils of carbon steel, structural steel, high-strength low-alloy steel, high-strength low-alloy steel with improved formability, and ultra-high strength steel. The specification covers steel sheet, strip, and coils in thicknesses less than 0.230 in. A1011 Commercial Steel Type B is produced to a specified chemical composition only.

    Available Dimensions

    Hide/Show specific columns Edit
    Select columns to display
      Grade Product type Thickness
      (inchesmm)
      Width
      (inchesmm)
      CS Type B Coils 0.188 - 0.2294.78 - 5.82 60 - 981500 - 2500
      Compare parameters

      Select one parameter to compare

      Comparison

        Chemical Composition

        (Heat analysis, wt %.)

        Hide/Show specific columns Edit
        Select columns to display
          Grade C
          (max wt %)
          Mn
          (max wt %)
          P
          (max wt %)
          S
          (max wt %)
          Ti 1)
          (max wt %)
          Cb
          (max wt %)
          Ni
          (max wt %)
          Mo
          (max wt %)
          Cu 2)
          (min wt %)
          Cr
          (max wt %)
          V
          (max wt %)
          CS Type B 0.15 0.60 0.03 0.035 0.025 0.008 0.20 0.06 0.20 0.15 0.008
          Compare parameters

          Select one parameter to compare

          Comparison

            1) For steels containing 0.02% carbon or more, Ti is permitted to the lesser of 3.4N + 1.5S or 0.025%.

            2) Copper steel with 0.20% minimum Cu.