ABS Grade AH36, DH36, EH36

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

    Show specs in Imperial Metric

    General Product Description

    ABS Grades AH36, DH36, and EH36 are higher-strength structural steels with a minimum specified yield strength of 51 ksi and specified minimum Charpy Vnotch impact toughness properties.

    Applications

    Typical applications include shipbuilding and mobile offshore drilling units and structures.

    Available Dimensions

    Hide/Show specific columns Edit
    Select columns to display
      Grade Product type Thickness
      (inchesmm)
      Width
      (inchesmm)
      Length
      (inchesmm)
      Grade AH36 Plate 0.1875 - 5.904.762 - 150 72 - 129.91800 - 3299 79 - 10202000 - 25910
      Grade DH36 Plate 0.1875 - 5.904.762 - 150 72 - 129.91800 - 3299 79 - 10202000 - 25910
      Grade EH36 Plate 0.1875 - 5.904.762 - 150 72 - 129.91800 - 3299 79 - 10202000 - 25910
      Compare parameters

      Select one parameter to compare

      Comparison

        Width: Please inquire for plate widths less than 72 in. and inquire plate product over 120 in.

        Length: Please inquire for plate lengths less than 240 in. and greater than the listed maximum.

        Mechanical Properties

        Tensile testing is performed in the transverse direction.

        Hide/Show specific columns Edit
        Select columns to display
          Grade Product type Thickness
          (inchesmm)
          Yield strength
          (min ksi)
          Tensile strength
          (ksi)
          Elongation A5 1)
          (min %)
          Grade AH36 Plate 0.1875 - 5.904.762 - 150 51 71 - 90 22
          Grade DH36 Plate 0.1875 - 5.904.762 - 150 51 71 - 90 22
          Grade EH36 Plate 0.1875 - 5.904.762 - 150 51 71 - 90 22
          Compare parameters

          Select one parameter to compare

          Comparison

            1) See ABS Rules for elongation requirements for alternative tensile specimens.

            Impact Properties

            Hide/Show specific columns Edit
            Select columns to display
              Grade Thickness
              (inchesmm)
              Test temperature
              (°F)
              Min Longitudinal Average Energy 1)
              (ft-lbs)
              Min transverse average energy 1)
              (ft-lbs)
              AH36 0.1875 - 2.004.762 - 50.8 32 25 17
              AH36 2.001 - 2.8050.83 - 71.1 32 30 20
              AH36 2.801 - 5.9071.15 - 150 32 37 25
              DH36 0.1875 - 2.004.762 - 50.8 -4 25 17
              DH36 2.001 - 2.8050.83 - 71.1 -4 30 20
              DH36 2.801 - 5.9071.15 - 150 -4 37 25
              EH36 0.1875 - 2.004.762 - 50.8 -40 25 17
              EH36 2.001 - 2.80050.83 - 71.12 -40 30 20
              EH36 2.801 - 5.9071.15 - 150 -40 37 25
              Compare parameters

              Select one parameter to compare

              Comparison

                1) Specimen orientation at the option of the manufacturer unless otherwise specified in the order.

                No more than one value below the specified miniminum average energy but no less than 70% of the specfied minimum average energy value.

                Minimum average energy for full-size specimens. Refer to ABS Rules for sub-size specimen energy requirements.

                Carbon Equivalent CET(CEV)

                Hide/Show specific columns Edit
                Select columns to display
                  Grade AH36 AH36 DH36 DH36 EH36 EH36
                  Thickness (inchesmm) 0.1875 - 2.004.762 - 50.8 2.001 - 3.0050.83 - 76.2 0.1875 - 2.004.762 - 50.8 2.001 - 3.0050.83 - 76.2 0.1875 - 2.004.762 - 50.8 2.001 - 3.0050.83 - 76.2
                  CEV 1) (max %) 0.38 0.40 0.38 0.40 0.38 0.40
                  Compare parameters

                  Select one parameter to compare

                  Comparison

                    1) Carbon equivalent requirements for TMCP condition of supply only.